Reducing surface recombination in black silicon photovoltaic devices using atomic layer deposition

Repo P.R.
Keywords:

black silicon, atomic layer deposition, surface passivation, photovoltaic devices

Document type Thesis
Journal title / Source
University name Aalto University
Publisher's name Unigrafia Oy
Publisher's address (city only) Helsinki
Publication date 2016-6-20
ISBN 978-952-60-6919-7
Web URL http://urn.fi/URN:ISBN:978-952-60-6919-7
Language English
Persistent Identifier http://urn.fi/URN:ISBN:978-952-60-6919-7